Investigation into the applicability of Bond Work Index …
The particle size range of the biomass particles (prior to densification) was obtained using the British standard BS EN 16126:2012 [39]. 2 litres of boiling deionised water was poured over 300 ± 1 g of each pellet sample and then soaked for 24 h. The samples were then dried at 35–60 °C until they reached 5–15% moisture content.The …